- Title
- Dry mechanochemical conversion of SrSO4 to SrCO3
- Creator
- Setoudeh, N.; Welham, Nicholas; Azami, S. M.
- Date
- 2010
- Type
- Text; Journal article
- Identifier
- http://researchonline.federation.edu.au/vital/access/HandleResolver/1959.17/41806
- Identifier
- vital:2627
- Identifier
-
https://doi.org/10.1016/j.jallcom.2009.11.114
- Identifier
- ISSN:0925-8388
- Abstract
- The effect of milling time on the dry conversion of celestite, SrSO4, to SrCO3 using sodium carbonate in a planetary type ball mill was investigated. After milling, the powders were leached in distilled water at room temperature and the solids then washed with 1 N HCl to separate the products. X-Ray diffraction analysis showed that SrSO4 started to transform to SrCO3 within 10 min of milling and the extent of conversion increased with milling time reaching >90% after 30 min. A <99% conversion of celestite to SrCO3 was obtained in 30 min by increasing the molar ratio of Na2CO3:SrSO4 to 1.3:1. © 2009 Elsevier B.V. All rights reserved.
- Publisher
- Elsevier
- Relation
- Journal of Alloys and Compounds Vol. 492, no. 1-2 (2010), p. 389-391
- Rights
- Copyright Elsevier
- Rights
- This metadata is freely available under a CCO license
- Subject
- 0912 Materials Engineering; 0914 Resources Engineering and Extractive Metallurgy; Celestite; Dry milling; Mechanochemistry; SrCO3
- Reviewed
- Hits: 883
- Visitors: 785
- Downloads: 2
Thumbnail | File | Description | Size | Format |
---|